Nikil fil-Pocket Mikro Capacitors Żommna Konnessi

Feb 21, 2022

L-ismartphone fil-but tiegħek huwa sistema elettronika kumplessa b'ħafna funzjonijiet differenti mħaddma mill-istess batterija integrata-.

Nickel in pocket micro capacitors keep us connected.jpg

An electronic circuit consists of independent electronic components, such as resistors, transistors, capacitors, inductors, and diodes, connected through wires or circuit boards. Capacitors have the ability to store charges, or "containers", much like small rechargeable batteries.

Fi prodotti tal-elettronika għall-konsumatur, ġeneralment ikun hemm mijiet ta' mikro-capacitors, u fi smartphones-high-end bħall-iPhone, hemm aktar minn 1000 mikro-capacitors. Dawn jissejħu capacitors taċ-ċeramika b'ħafna-saffi (MLCC), li jistgħu jkunu żgħar daqs ħbub tar-ramel fuq il-bajja tal-vaganzi favorita tiegħek. Il-funzjoni tagħhom hija li jiddiżakkoppjaw is-subcircuit mill-varjazzjoni tal-qawwa kkawżata mill-attività ta 'subcircuit ieħor.

In-nikil inaqqas id-daqs tal-MLCC billi jnaqqas il-ħxuna tas-saff tal-insulazzjoni u jżomm il-kapaċità kostanti. Fl-2020, 4800t trab tan-nikil intuża biex jipproduċi MLCC ta' daqs-ramel.