Titanju Għal Tagħmir tal-Baħar

Mar 02, 2022

Titanium alloy can not only make marine equipment develop towards "deep, large, far, high ", but also fully realize the same life as the main body of marine equipment. It is the best choice for marine equipment. At present, China pays more attention to the application of titanium in marine equipment, and the amount of titanium used is also increasing. Deep-sea pressure shell, seawater pipeline, cylinder superstructure, frame, etc. will become the key development direction of marine titanium.

marine equipment

Fil-preżent, hemm ħafna applikazzjonijiet tat-titanju fl-industrija tat-tbaħħir fid-dar u barra.

However, the material system in relevant specifications is not perfect. It is hoped that relevant units will organize discussion and improve the material system in current relevant codes such as Titanium Pressure Vessel, Material and Welding, so as to facilitate the designer's reference.

Upper buildings: 

Fil-preżent, hemm xi eżempji ta 'applikazzjoni fis-sovrastruttura domestika tal-vapuri tal-gwerra, bħal Ti70 (TA23) għall-arblu, TA5 u TA7 bar għall-antenna tar-radar, pjanċa TA2 u TA5 għall-ġilda tal-hangar, u struttura tal-qafas.

It-titanju jintuża wkoll b'mod estensiv fiż-żoni tal-bini ta 'fuq tal-vapur tat-trasport tal-baċir anfibju LPD17, inaqqas il-massa tiegħu b'madwar 50 fil-mija u jtejjeb ħafna l-istabbiltà tiegħu.

Applikazzjonijiet ta' Produzzjoni f'Oqsma Oħra

Minbarra ammont kbir ta 'titanju użat fid-djar reżistenti għall-pressjoni ta' hawn fuq-, sistema ta 'pajpijiet, u sovrastruttura, komponenti oħra huma wkoll utli f'tagħmir tal-baħar fid-dar u barra.